CSIRO - TEST REPORTS
Return to Home Page

CONSOLIDATED TILING SERVICES

21 November 2000

Our Ref. EN 13/713

TEST REPORT No. 1782

Requested by: Tasco Brick Block & Pavers

On: 21 November 2000

Manufacturer: Tasco Brick Block & Pavers

Product Desc. Tasco Tech-Dry Concrete Masonry Unit

Tasco Tech-Dry Mortar

Product size 110mm x 228mm x 75mm

Sampling details:

Where: Delivered

Date: 21 November 2000

By whom: Tasco

How (methods): N/A

The results reported relate only to the sample(s) tested.

No responsibility is taken for the accuracy of the sampling unless it is done under our own supervision.

The reproduction of this test report is only authorised in the form of a complete photographic facsimile. Our written approval is necessary for any partial reproduction.

SUMMARY OF TESTS PERFORMED:

Test based on AS 3700 – 1988

Flexural Strength by Bond Wrench Average: 0.449 MPa

Report No. 1782

Flexural Strength by Bond Wrench Test

TEST BASED ON AS 3700 – 1988

Samples received 15 November 2000 Test Date 21 November

Flexural Strength
Sample No. Mpa

1. 0.357

2. 0.260

3. 0.589

4. 0.426

5. 0.627

6. 0.371

7. 0.308

8. 0.445

9. 0.430

10. 0.681

Average 0.449

Interpretation of results: The Tasco Tech-Dry Masonry Unit with Tech-Dry Mortar show a close and continuous range for the Flexural Strength test . The average of 0.449 Mpa is considered a high result for masonry products.

Date and Place 21 November 2000, Highett, Vic.


BARRY SCHAFER - APPRAISALS MANAGER

PETER WESTGATE - SENIOR LABORATORY TECHNICIAN